Hydrolysis of dicalcium phosphate dihydrate in a sodium acetate solution , издательство Pleiades Publishing, Ltd (Road Town, United Kingdom), том 447, с. 303-305 DOIстатья
Статья опубликована в журнале из списка Web of Science и/или Scopus
Дата последнего поиска статьи во внешних источниках: 4 марта 2022 г.
Местоположение издательства:Road Town, United Kingdom
Первая страница:303
Последняя страница:305
Аннотация:Depending on the time of hydrolysis at pH 6.8 and 37 C, the following compounds are identified by pow der X ray diffraction (table). During the first 14days, single phase OCP is formed. The CSL calculated for DCPD decreases from 92 to 57 nm and an amorphous component (20 wt%) appears (table). The CSL for OCP on the 14th day reaches the maximum value of 50 nm. Octa calcium phosphate has a needle crystalmorphology, unlike DCPD, which has plate crystals (Fig. 1). On further OCP hydrolysis, OCP